TP004 - Effect of Copper on Active Dissolution and Pitting Corrosion of 25%Cr Super Duplex Stainless Steels
Download PDF (opens in new tab)

This paper is a clear demonstration of how elevated copper additions improve pitting resistance.

It compares Ferralium® 255 with other duplex alloys that have less optimised compositions, showing the benefit of the higher copper content.